Someone recommends the use of PIPE LONGITUDINAL SEAM to the following conditions:

Design Pressure: 1500 psi
Gas volume: 1500 MMPCND
H2S: 12 ppm
CO2: 7-8% molar
H2O: 5 lb / MMPCND
Material pipe: API 5L X70

reggards
 
OK, was there a question there?

David
 
with the conditions mentioned above, there is someone to recommend the use of pipes with longitudinal seams?
 
Welded API 5LX-70 is most often specified for similar service conditions.

 