enginesrus
Mechanical
- Aug 30, 2003
- 1,026
I don't ever remember hearing such things happening through the 1960's to the 1990's.
This is very dangerous, I hope it all gets sorted soon.
It sounds like a materials issue of some sort.
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
CWB1 said:Out of curiosity I did a quick search on NHTSA's site for steering system recalls 1970-1980. Data prior to 1970 is scarce, prob bc NHTSA was formed in 1970. Note, I haven't used their system in years and in certain circumstances recalls will actually be listed under the component supplier rather than the OEM, so I prob missed a LOT.
PACCAR brands had steering recalls in 1971, 72, 73, 74, 76, 78, and 79.
Mack had steering recalls every year from 1970-1980. Volvo only had one that I was able to locate in 1980.