Guest
Can anyone give me where I can get the solution strength for commercial ferric chloride?

Thanks in advance
 
Am sure there must be several chemical suppliers in your yellow pages but one of the top notch suppliers of inorganic coagulants such as Ferric Chloride across North America, and Latin America is Eaglebrook Inc. US phone # 1-800 428 3311 or look at Good hunting
 
Typical analysis of Ferric Chloride:

specific gravity = 1.40 - 1.50
FeCl3 % w/w = 40 - 45

undesired components:
FeCl2 % w/w < 0.5 - 0.1
HCl % w/w < 0.5 - 0.1

unaceptable components:
Cr(VI) & heavy metals

Regards,
LS

 