May 16, 2002 #1 Guest Can anyone give me where I can get the solution strength for commercial ferric chloride? Thanks in advance
Can anyone give me where I can get the solution strength for commercial ferric chloride? Thanks in advance
May 20, 2002 #2 PBroad Mining Joined Mar 27, 2002 Messages 113 Location CA Am sure there must be several chemical suppliers in your yellow pages but one of the top notch suppliers of inorganic coagulants such as Ferric Chloride across North America, and Latin America is Eaglebrook Inc. US phone # 1-800 428 3311 or look at http://www.eaglebrook.netGood hunting Upvote 0 Downvote
Am sure there must be several chemical suppliers in your yellow pages but one of the top notch suppliers of inorganic coagulants such as Ferric Chloride across North America, and Latin America is Eaglebrook Inc. US phone # 1-800 428 3311 or look at http://www.eaglebrook.netGood hunting
May 24, 2002 #3 luissabate Chemical Joined May 24, 2002 Messages 12 Location AR Typical analysis of Ferric Chloride: specific gravity = 1.40 - 1.50 FeCl3 % w/w = 40 - 45 undesired components: FeCl2 % w/w < 0.5 - 0.1 HCl % w/w < 0.5 - 0.1 unaceptable components: Cr(VI) & heavy metals Regards, LS Upvote 0 Downvote
Typical analysis of Ferric Chloride: specific gravity = 1.40 - 1.50 FeCl3 % w/w = 40 - 45 undesired components: FeCl2 % w/w < 0.5 - 0.1 HCl % w/w < 0.5 - 0.1 unaceptable components: Cr(VI) & heavy metals Regards, LS