Hi,
How best is it to cast a polymer resin solid surface sheet?
 
Replies continue below

Recommended for you

I think you mean to cast a resin into smooth hard surface sheets. If so, cell cast between sheets of glass is the traditional method of making acrylic sheet like Perspex.

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
If you want advice on solid surfaces i.e. synthetic stone counter tops, then I can put you in touch with a world-class expert who developed those materials.