Solid solution alloying vs precipitation hardening

Status
Not open for further replies.

waqasmalik

Mechanical
Joined
Jul 18, 2013
Messages
177
Location
PK
Hi all, can anyone please tell me what is the basic difference between solid solution alloying and precipitation hardening? Which and these methods can be used for strengthening of various commonly used materials like low carbon steels, austenitic stainless steels and 2000 series of aluminium?


Thanx in advance
 
Do you have a Physical Metallurgy on hand? Please read it.


"Even,if you are a minority of one, truth is the truth."

Mahatma Gandhi.
 
If it is a single phase material then it must be solution strengthened (autenitic stainless).
If there are multiple phases then it is either a precipitation mechanism or a transformation mechanism.
Pick up a copy of PM by Reed-Hill.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 