msmamma

Materials
Jul 9, 2009
1
I am trying to come up with a transparent medium in which to incorporate scatters and dye and make a solid phantom. I cannot find an epoxy to use that is optically clear nor a standard that can be removed from a mold. Any suggestions?
 
Replies continue below

Recommended for you

Don't people normal use acryllic for this?

TTFN

FAQ731-376
 
Yes they do.

Acryic casting resins also known as methyl methacrylate casting resins.

Regards
Pat