BY USING ROTERS I DESIGNED A SOLENOID WITH CENTER PLUNGER AND OUTSIDE SHELL TO COMPLETE THE MAGNETIC CIRCUIT. THIS SOLENOID GETS 3 AMP PULSE AT 25 HZ. IT PRODUCES 50 POUNDS
FORCE. IT'S AN ELECTRIC HAMMER. IT'S CONSTRUCTED FROM CMI-C IRON AND HAS A COOLING FAN TO CONTROL THE TEMPERATURE.
SO FAR SO GOOD.
WE NEED THIS SOLENOID TO RUN 500 HOURS. WE HAVE A TEST STAND WHERE WE CYCLE IT AGAINST A 10 POUND SPRING. RUNS AT ABOUT 100 C AND 100 V BEAUTIFULLY FOR ABOUT 10 OR 15 HOURS. QUITS ABRUPTLY.
ELECTRICAL PULSE TRAIN IS THERE. WE THOUGHT WE HAD SHORTED TURNS IN THE COIL, BUT THE COIL IS PERFECT AFTER 15 HOURS. WE ADDED "HEAVY" INVERTER INSULATION ON THE WIRE. STILL FAILED IN LESS THAN 20 HOURS.
ONE DAY ON LOOKING AT A FAILED UNIT, I DECIDED TO CHANGE THE PLUNGER. POWER RETURNED. I'VE RETURNED TO ANNEALING THE IRON BEFORE ASSEMBLY WHICH IS DONE TO INCREASE MAGNETIC FLUX. WE HAVE PLENTY OF MAGNETIC HIT SO I HAD GIVEN UP ANNEALING THE PARTS. WILL TEST THE ANNEALED ASSEMBLIES NEXT WEEK BUT I DON'T HAVE ANY GREAT HOPE THAT THIS WILL RESOLVE THE PROBLEM.
QUESTION; IS THERE A BETTER ALLOY CHOICE TO RESIST VIBRATION AND IMPACT. THE TEMPERATURE IS ONLY 100 C, BUT THE 50 POUND IMPACT AT 25 HZ MIGHT BE CHANGING THE GRAIN STRUCTURE. THE PLUNGER DIAMETER IS ABOUT 1.0". IT LANDS ON RUBBER PADS AT EACH END, BUT SOUNDS LIKE AN AK47 WHEN IT'S RUNNING.
THANKS FOR ANY IDEAS, WE'RE OUT.
JIM (MECHANICAL)
FORCE. IT'S AN ELECTRIC HAMMER. IT'S CONSTRUCTED FROM CMI-C IRON AND HAS A COOLING FAN TO CONTROL THE TEMPERATURE.
SO FAR SO GOOD.
WE NEED THIS SOLENOID TO RUN 500 HOURS. WE HAVE A TEST STAND WHERE WE CYCLE IT AGAINST A 10 POUND SPRING. RUNS AT ABOUT 100 C AND 100 V BEAUTIFULLY FOR ABOUT 10 OR 15 HOURS. QUITS ABRUPTLY.
ELECTRICAL PULSE TRAIN IS THERE. WE THOUGHT WE HAD SHORTED TURNS IN THE COIL, BUT THE COIL IS PERFECT AFTER 15 HOURS. WE ADDED "HEAVY" INVERTER INSULATION ON THE WIRE. STILL FAILED IN LESS THAN 20 HOURS.
ONE DAY ON LOOKING AT A FAILED UNIT, I DECIDED TO CHANGE THE PLUNGER. POWER RETURNED. I'VE RETURNED TO ANNEALING THE IRON BEFORE ASSEMBLY WHICH IS DONE TO INCREASE MAGNETIC FLUX. WE HAVE PLENTY OF MAGNETIC HIT SO I HAD GIVEN UP ANNEALING THE PARTS. WILL TEST THE ANNEALED ASSEMBLIES NEXT WEEK BUT I DON'T HAVE ANY GREAT HOPE THAT THIS WILL RESOLVE THE PROBLEM.
QUESTION; IS THERE A BETTER ALLOY CHOICE TO RESIST VIBRATION AND IMPACT. THE TEMPERATURE IS ONLY 100 C, BUT THE 50 POUND IMPACT AT 25 HZ MIGHT BE CHANGING THE GRAIN STRUCTURE. THE PLUNGER DIAMETER IS ABOUT 1.0". IT LANDS ON RUBBER PADS AT EACH END, BUT SOUNDS LIKE AN AK47 WHEN IT'S RUNNING.
THANKS FOR ANY IDEAS, WE'RE OUT.