dantheman76
Materials
I cannot seem to find information on silver soldering to 154CM stainless.
I'm a knive maker and I need stats on this process if it is possible. Manly so I don't over temper my blade in the process.
Thanks
I'm a knive maker and I need stats on this process if it is possible. Manly so I don't over temper my blade in the process.