I'm looking for a current industry spec similar to DOD-STD-1866 which is inactive. What is presently used for metal joining e.g. sheet metal?
 
Replies continue below

Recommended for you

You can look at the following:

ASTM B 32
Revision: 04 Chg: Date: 11/01/04
STANDARD SPECIFICATION FOR SOLDER METAL

ISO 9453
Revision: 90 Chg: Date: 12/01/90
SOFT SOLDER ALLOYS - CHEMICAL COMPOSITIONS AND FORMS

AWS SHB
Revision: 3RD Chg: Date: 00/00/00
SOLDERING HANDBOOK




 