Hi Guys,
I am working on a project that requires reviewing some soil resistivity data. The values I've got are around 800,000 ohms-cm, they were measured in damp to moist silty, clayey sands. They seemed pretty high, are these values possible? I have read literatures suggesting that the maximum values are around 500,000 ohms-cm. Where could I find some sound references?
Thanks for your help!
I am working on a project that requires reviewing some soil resistivity data. The values I've got are around 800,000 ohms-cm, they were measured in damp to moist silty, clayey sands. They seemed pretty high, are these values possible? I have read literatures suggesting that the maximum values are around 500,000 ohms-cm. Where could I find some sound references?
Thanks for your help!