Soil lifts and compaction schedule for solid sand under a slab on grade home 4" conc floor? Home will have CMU frost walls.
Building a 2700 sq ft home. Using 4" conc floor and radiant hydronic heat with tubes in the concrete. My spec for the floor is the following, what if anything can or should be changed or is this JUST FINE?!
4" conc floor 4,000 psi mix
4" Type XIV EPS foam insulation, 6 mil PE beneath to prevent R value devaluation (. . . How about above it too??)
4" x 3/4" clean stone
8" compacted ABC class six to native material
6" native material
I copied this spec from another home drawing but it is probably either over or under specified for MY soil.
My soil is almost pure sand. I used a 20" auger on my track loader and got down 4 ft before running out of shaft length. EVERYTHING looked the same-- beautiful clean sand. Location: Sherburne County Minnesota, land is ON the ELK River, home site location on a hill 25 ft above the river plain and 200 yd from river itself.
My excavator questioned the need for the ABC class six. What do you guys think?
Building a 2700 sq ft home. Using 4" conc floor and radiant hydronic heat with tubes in the concrete. My spec for the floor is the following, what if anything can or should be changed or is this JUST FINE?!
4" conc floor 4,000 psi mix
4" Type XIV EPS foam insulation, 6 mil PE beneath to prevent R value devaluation (. . . How about above it too??)
4" x 3/4" clean stone
8" compacted ABC class six to native material
6" native material
I copied this spec from another home drawing but it is probably either over or under specified for MY soil.
My soil is almost pure sand. I used a 20" auger on my track loader and got down 4 ft before running out of shaft length. EVERYTHING looked the same-- beautiful clean sand. Location: Sherburne County Minnesota, land is ON the ELK River, home site location on a hill 25 ft above the river plain and 200 yd from river itself.
My excavator questioned the need for the ABC class six. What do you guys think?