Hello to all,
would you recommend me a software related material selection for line pipe on sweet and sour service?
regards
Peter
 
Replies continue below

Recommended for you

Peter

There are some good software for Corrosion prediction in sweet and sour service.
The Norsok software is free, but is limited to a Sweet service, there is a limit on the max H2S. You can download it at:

Then there are others software that you can try and buy.
The electronic engineer from intetech can take into account also the effect of h2s on corrosion:

hope this help u

S.


 