Hi all.
I have a few cold drawn sae 9260 round bar , size from 7/16" (11,11 mm) to 3/4" (19,05 mm) and I need to down its hardeness to less than 190 brinnel.
What could be the appropiate heat treatment .?
The pourpouse of this treatment is to allow a cold drawn reduction to get smaller diameter.
The material will be used to make car suspension springs, it will hardendened after coiling .
This the chemical composition
Component
Carbon, C 0.56 0.64
Iron, Fe 96
Manganese, Mn 0.88
Phosphorous, P 0.035
Sulfur, S 0.04
Silicon, Si 2
Thanks in advance Pardal
I have a few cold drawn sae 9260 round bar , size from 7/16" (11,11 mm) to 3/4" (19,05 mm) and I need to down its hardeness to less than 190 brinnel.
What could be the appropiate heat treatment .?
The pourpouse of this treatment is to allow a cold drawn reduction to get smaller diameter.
The material will be used to make car suspension springs, it will hardendened after coiling .
This the chemical composition
Component
Carbon, C 0.56 0.64
Iron, Fe 96
Manganese, Mn 0.88
Phosphorous, P 0.035
Sulfur, S 0.04
Silicon, Si 2
Thanks in advance Pardal