Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Soft, temperature-resistant gasket for use in reactor 1

Status
Not open for further replies.

Broblawsky

Materials
Joined
Jun 8, 2005
Messages
1
Location
US
I'm trying to set up a reactor that uses a pair of ceramic plates. In order to make sure no gas escapes, I need to install a gasket. However, this system sandwiches a piece of brittle carbon paper between two ceramic plates, which are then screwed together. I need a gasket which can a) withstand temperatures up to 600-700 C and exposure to carbon monoxide, and b) is soft enough to avoid cracking the brittle carbon paper or the ceramic plates when they are screwed together. The pressure shouldn't be much above normal room pressure, so the seal doesn't have to be that strong. Your help would be much appreciated.
 
Trying Garlock 1-800-448-6688. They're very helpful.

 
Garlock won't have any suitable gasket materials for 600C. If you have low pressure, you should use a ceramic paper (felt) gasket. Look at the FiberFrax website for more info. We use this material for hot exhaust gases on flimsy ductwork flanges with low bolting and it works very well.
 
Status