Plant standards call for the use of 316SS Graphite Laminate Gaskets for 46% Sodium Hydroxide storage and distribution system.
Has anyone had experience with this type of gasket material in similar service conditions?
Medium: 46% Sodium Hydroxide
Temperature: 50 Deg. C max
Pressure: 300 kPa (44 PSI)
Has anyone had experience with this type of gasket material in similar service conditions?
Medium: 46% Sodium Hydroxide
Temperature: 50 Deg. C max
Pressure: 300 kPa (44 PSI)