What is the min allowable pipe to fitting engagement for a socket weld?
Thanks
Sftyvlv
 
Replies continue below

Recommended for you

ASME B31.1 also has information about the proper fit-up for socket welded joints.

The general idea is to leave ~1/16" inch gap at the bottom of the joint to allow for weld shrinkage.

-MJC

 