Good Morning All

Which ASME standard I have to use to check the end-to-end or face-to-face dimension for Class 150 2" Skocet-weld end valve?

Thanks
 
API 602/ISO 15761, clause 5.4.2.4 states that end-to-end dimensions of socket-welding valves shall be established by the manufacturer.
 
Also, in regards to an ASME spec; ASME B16.34-2009 section 6.2.6 states that any valve type not included in ASME B16.10 (which socket weld is NOT covered in) for End-To-End dimensions shall be the manufacturer's standard.
 