What kind of weld would be a better option, a butt weld or a socket weld on an 1 13/16" -10,000 psi API flange (super duplex UNS S32750) to a 1" ID tube, 0.118" tk strangely thin!!!(super duplex UNS S32750) which is also rated to 10,000 psi. The assembly has to be rated to 10,000 psi

Thank you for the time
 
Replies continue below

Recommended for you

I prefer butt weld with RT 100%.
 
I think if you talk with the welders (the people that have to DO the work); you find that they prefer to do the socket weld in that size. Would be a way easier procedure!
 