I would like to know if its normal to have a Leak in a Test during filling conditions, but in pressure is complete LEak proof.
Imean, i am testing a 24 inch PVC pipe with gasket joint 1000 Ft lenght. During filling we detect small leaks in 4 joints, but once the pipes gets just a little pressure (about 35 PSI) the leak stops and pass the 2 hours test ay 150 PSI with no problem. The main problem now is that the inspection is killing me with questiong regarding to if this is normal. A couple of PVC pipe manufacturer told me that its perfectly normal, but when i ask to a document (standard, essay, textbook or something) they told me that there isn't any. It's this true? where i can find info about it if this is possible
Thank you ! i have only 2 days to answer to the inspection before they consider the test as Fail!.
Regards,
Imean, i am testing a 24 inch PVC pipe with gasket joint 1000 Ft lenght. During filling we detect small leaks in 4 joints, but once the pipes gets just a little pressure (about 35 PSI) the leak stops and pass the 2 hours test ay 150 PSI with no problem. The main problem now is that the inspection is killing me with questiong regarding to if this is normal. A couple of PVC pipe manufacturer told me that its perfectly normal, but when i ask to a document (standard, essay, textbook or something) they told me that there isn't any. It's this true? where i can find info about it if this is possible
Thank you ! i have only 2 days to answer to the inspection before they consider the test as Fail!.
Regards,