Hi,
I need some advice on how to enlarge some current holes in a 41340 steel part.
The part is a plate with a series of small hole in, varying from 0.030" through to 0.060". The person who designed it, who is no longer working for us, had the machinist drill the holes using a regular drill bit. But unfortunately they are the wrong size holes and we believe some of the holes aren't concentric.
We'd like to open up these holes by on average 0.015", as the size is very important for its application.
Could anyone suggest a method of opening these holes up?
I have had limited experience with EDM, but do not know if it is capable of opening up an existing hole to this particular accuracy. We'd like the holes to within 0.0005" of their designed spec. if possible? IS EDM suitable? Are there any other more efficient methods?
Cheers,
Michael
I need some advice on how to enlarge some current holes in a 41340 steel part.
The part is a plate with a series of small hole in, varying from 0.030" through to 0.060". The person who designed it, who is no longer working for us, had the machinist drill the holes using a regular drill bit. But unfortunately they are the wrong size holes and we believe some of the holes aren't concentric.
We'd like to open up these holes by on average 0.015", as the size is very important for its application.
Could anyone suggest a method of opening these holes up?
I have had limited experience with EDM, but do not know if it is capable of opening up an existing hole to this particular accuracy. We'd like the holes to within 0.0005" of their designed spec. if possible? IS EDM suitable? Are there any other more efficient methods?
Cheers,