Mar 23, 2005 #1 kthomas Industrial Joined Nov 7, 2004 Messages 7 Location FI Does somebody know manufacturer of wet sieves? Sieve would become to take too big agglomerates away from water-ceramicpowder-slurry. Sieve size should be around 200µm. Amounts to be sieved is not big.
Does somebody know manufacturer of wet sieves? Sieve would become to take too big agglomerates away from water-ceramicpowder-slurry. Sieve size should be around 200µm. Amounts to be sieved is not big.
Mar 25, 2005 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US Give these people a call. http://www.sweco.com/ There are several manufacturers of this type equipment. Upvote 0 Downvote
Give these people a call. http://www.sweco.com/ There are several manufacturers of this type equipment.
Mar 28, 2005 #3 itdepends Chemical Joined Sep 16, 2004 Messages 236 Location AU An alternative http://www.kason.com Upvote 0 Downvote