Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Slip-on flange external fillet weld size of Figure UW-21 and Figure 2-4

Status
Not open for further replies.

mechengineer

Mechanical
Joined
Apr 19, 2001
Messages
268
Location
SG
The external weld leg size = Xmin=1.4tn from Fig. UW-21.
The external weld leg size = c = tn from Fig. 2-4.
This looks like double stands and confused. And this may virtually make a contradiction between the client/user and manufacturer. The manufacturer prefers Fig. 2-4, but client may prefer Fig.UW-21.

 
 http://files.engineering.com/getfile.aspx?folder=1b6fd116-a042-4672-a3f8-d7d679c9e241&file=Capture.JPG
mechengineer, here's the key: "When ASME B16.5 slip-on flanges are shown to comply with all the requirements provided in Mandatory Appendix 2 of this Division..."

They rarely do. Subject is discussed frequently, try a site search for more detail.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 