I have a cylindrical assembly that I need to bond together. One side is a thin walled 3AL 2.5V tube, the other side wil be 7075 alloy. I would prefer to anodize the 7075 throughout, but I can have the outer edges masked. My diameter between my slip fit parts is roughly 32mm. My depth is about 23mm. I can hold close tolerances. I was planning on a light press fit with a bonding agant.
The assembly will see mainly radial loads, but I do have an overhanging load that will be no more than 1400 lbs. My stresses are cyclic and could be reversed also.
I talked with a Loctite tech supprt engineer, and they suggested loctite 609. I have had a lot of luck with this type of bonding agent, but I would prefer to use 638 for its higher strength. Loctite admittedly hadnt tested this, so their suggestion was a guess.
Anyone out there with a similar situtaion or another adhesive that can give me over 3000 psi shear on aluminum?
Also, I was planning on calling out a 64 RMS finish on my parts. Anyone have a suggestion as to whether this can work for me r not?
Thanks
Dave
The assembly will see mainly radial loads, but I do have an overhanging load that will be no more than 1400 lbs. My stresses are cyclic and could be reversed also.
I talked with a Loctite tech supprt engineer, and they suggested loctite 609. I have had a lot of luck with this type of bonding agent, but I would prefer to use 638 for its higher strength. Loctite admittedly hadnt tested this, so their suggestion was a guess.
Anyone out there with a similar situtaion or another adhesive that can give me over 3000 psi shear on aluminum?
Also, I was planning on calling out a 64 RMS finish on my parts. Anyone have a suggestion as to whether this can work for me r not?