Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Slip Coefficient of Mechanicaly Polished Concrete

Status
Not open for further replies.

mseely01

Structural
Joined
Nov 4, 2009
Messages
2
Location
US
Does any one know the slip coefficient of concrete once hardened and sealed using a mechanical grinding and polishing process?
 
Not something you can guess. It depends on the level of polish, the porosity of the concrete, the aggregate type...etc. It will make a difference whether it is wet or dry, as well.

Easier to test it and then you'll know. Assuming you are in the US, it can be field tested for about $150.
 
Ron is right, but BS8110 gives friction coeff't of 'smooth interface, as in untreated concrete' to be 0.7.
Polished concrete is bound to be less than that.
 
From the research I have done it turns out that by polishing the concrete you are creating a more dense surface. Therefore the coefficient increases and you have a more abrasive resistant flooring and a more slip resistant flooring than natural or raw concrete. I still dont have any numbers as to what it is but they are saying it increases by a minimum of 10%
 
mseely01....I have tested numerous floors and have found the opposite to be true. The coefficient of friction goes down as the roughness is reduced. For polished floors, I would expect the COF to be slightly more than 0.50 in the dry condition and less than that for the wet condition.
 