I've been looking in McMaster-Carr for grease. Frankly I'm dazed and confused.
I have some two ton, internal screw, jacks that have steel acme-threads with steel nuts, and some bevel gears to turn the horizontal rotating shaft motion into vertical acme thread motion. They are square, telescoping, tube-type jacks.
I have used lithium spray greases and been horrified to find the result dry and ungrease like in about a year. I have gotten Teflon based lubes that seem to be gone in a few months. Other greases seem to separate and the liquid part runs away leaving dried peanut butter.
These jacks will be put in service and can never be internally greased ever again. Whereas the exterior sliding parts could be. The life of these jacks is going to be directly related to the long term functionality of the grease I use.
Temperature will be normal ambients. Cycles will be infrequent.
It would be nice to use something that works on the slides and the internals. Barring that they would need to coexist as they could mix.
What can you suggest?
Keith Cress
kcress -
I have some two ton, internal screw, jacks that have steel acme-threads with steel nuts, and some bevel gears to turn the horizontal rotating shaft motion into vertical acme thread motion. They are square, telescoping, tube-type jacks.
I have used lithium spray greases and been horrified to find the result dry and ungrease like in about a year. I have gotten Teflon based lubes that seem to be gone in a few months. Other greases seem to separate and the liquid part runs away leaving dried peanut butter.
These jacks will be put in service and can never be internally greased ever again. Whereas the exterior sliding parts could be. The life of these jacks is going to be directly related to the long term functionality of the grease I use.
Temperature will be normal ambients. Cycles will be infrequent.
It would be nice to use something that works on the slides and the internals. Barring that they would need to coexist as they could mix.
What can you suggest?