In tunnel lining what does the term "slick line" mean
 
I should add it is a term used in a US standard in connection with placing concrete.
 
Slickline is metal pipe through which concrete is pumped. It's used to differentiate pipe from rubber hose that's used at the discharge end of large-diameter pumplines or from rubber hose that's used for the entire line of small-line pumps.
 