arash66
Materials
- Sep 3, 2009
- 16
I have been always told that if you get proof failure one of the main reasons can be slack quenching.
my questions are:
- is this true?
- what else can be involved?
- can we explain the reasons scinetifically (by dislocation theory or...)?
thank you evryone for your help.
my questions are:
- is this true?
- what else can be involved?
- can we explain the reasons scinetifically (by dislocation theory or...)?