How many of you have used a slab on grade without any reinforcing at all? We did this on one project and I am not aware of any problems resulting from it. I have discussed doing this before with a concrete professor/engineer who thinks this is the best way to go (referring to slabs with warehouse type loads or less on decent soil). His thought is that the wwf that normally ends up on the bottom of the slab due to the highly ineffective pull-up method does more harm than good.
That is, use a better mix and tighter control joint spacing and leave out the reinforcing completely.