We are building a slab on grade in the Caribbean where the Geotech Engineer has specified a potential free heave of 5”, a differential heave of 2.5” and an edge distance of 1.5m. The area is classified as very stiff to hard clays in a warm tropical climate with extreme dry and wet seasons. If I understand correctly the edge distance is the area of influence in the slab on grade that is likely to be exposed to a free heave of 5” if nothing is done to mitigate it. It means that the slab that is beyond this 1.5m edge distance (or internal slab) is not exposed to the heave as outlined above. However, the geotech engineer has suggested we find a way to stop the transfer of surface water into this 1.5m active zone around the edge of the slab on grade in which case we would mitigate the edge of the slab from heaving which ultimately means designing the slab as a simple slab on grade instead of a suspended slab.
Questions:
1. Has anybody seen such a design where the edge or active zone is the only potential area of concern since it is expected that water will move in and out of this zone depending on the season.
2. Any tips on how to mitigate this edge water. One suggestion was to excavate the active zone, which was specified as 3m below the slab on grade, and replace with concrete or some water stop.
3. Is 5” of heave realistic?
4. Should we be concerned about the free heave at the centre of the slab. In other words, it is likely that only this 1.5m edge area has the potential to heave 5” and not the centre of the slab. The water table is 1.5m below slab on grade and 1.5m of backfill at 95% compaction has been placed under the slab on grade.
5. Any good references or guidebooks that I can read up on for slab on grade/heave etc in warm temperate climates.
Questions:
1. Has anybody seen such a design where the edge or active zone is the only potential area of concern since it is expected that water will move in and out of this zone depending on the season.
2. Any tips on how to mitigate this edge water. One suggestion was to excavate the active zone, which was specified as 3m below the slab on grade, and replace with concrete or some water stop.
3. Is 5” of heave realistic?
4. Should we be concerned about the free heave at the centre of the slab. In other words, it is likely that only this 1.5m edge area has the potential to heave 5” and not the centre of the slab. The water table is 1.5m below slab on grade and 1.5m of backfill at 95% compaction has been placed under the slab on grade.
5. Any good references or guidebooks that I can read up on for slab on grade/heave etc in warm temperate climates.