First of all, it sounds like you want to design a pavement, not just a slab on grade. Further, it sounds like it might be an apron in front of a hangar or perhaps even a hanger floor slab.
If it is a pavement, design it as such. You will need to know wheel loadings and load frequency. For concrete you generally design so that the tensile stress at the bottom of the slab does not exceed 50% of the modulus of rupture of the concrete...then you don't have to worry too much about the number of load repetitions.
If it is a hangar slab, design everything but the integral footings as a pavement and then design the integral footings for the building loads...then tie the two together, considering lateral thrust resistance as well.
The US Army Corps of Engineers has some pretty good info on concrete pavement design for aircraft.