bvelazquez
Structural
I believe this should be an easy one for you all. I am locating a PVC 4"-diameter pipe underneath a slab on grade in a loading dock area. The PVC pipe will be approximately 12 inches below the slab on grade which is approximately 6 inches thick for a total of 18 inches below the loading point. How do I determine what schedule of pipe I need in order to resist the bearing pressure from a forklift or other heavy vehicle that transmits through the concrete slab into the compacted fill and eventually over the pipe? By the time the load is transmitted to the top of the pipe, I've got about 800 psf of bearing pressure. Any sugggestions on determining schedule of pipe?