Hi all,
I will set up a welding performance qualification for FCAW, double-welded groove weld. I am trying to study ASME IX but I am not sure I can get it all. So can you pls advice me size of test coupon (plate) for welder qualification per ASME IX. Thanks all.
 
Replies continue below

Recommended for you

Keep studying ASME IX.
If you cannot understand the code how can you qualify welders in accordance with the code ?
 
Ditto.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
Thanks. Does anybody help me with this? I hope that somebody will show me which clause in ASME IX that I can refer/study.
 
There are pictures in ASME IX that describe qualification test plates. Look at them.
 
I would start at QG-100.

If you're a vendor, you should contact your client for guidance.
 