I would like to tap a 6mm thread into a few short risers of aluminium round bar. What size round bar would I need to ensure the integrity of the round bar. Is there a minumum or standard to follow; e.g. the thickness of the wall must be at least x.

This is only for a custom dashboard and will hold a very small weight of 2mm aluminium plate so it is not structural.

I have attached a diagram if it posts ok.

Many thanks
Thierry
 
Replies continue below

Recommended for you

For non-structural, you could use 1.5 times the thread size as the bar outer diameter.
 
Wow!! That was a very quick response and the information is exactly what I was after. I will go with a 3/8" (9.5mm) round bar.
Many thanks to both for the information, much appreciated.
 