Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Site tesitng of Impressed current anodes before installation

Status
Not open for further replies.

elecsun

Electrical
Joined
Jul 12, 2004
Messages
16
Can someone explain in detail what are the field tests which can be carried to confirm anode material(We are using imressed current anodes for tank bottm protection-mixed metal oxide anodes)before installtion.i know we can get the material confirmation certificates from manufucturer. Whats are the simple field tests which confirm the quality of anode materials?
 
I supose that with a PMI (Positive Material Identification) you can confirme material composition of anode materials.
 
I'm confused.

I would want to confirm the material composition of SACRIFICIAL anodes.

I have not heard of confirming the material of an IMPRESSED CURRENT anode. Instead, I merely ensure the purchase spec is properly written. I do care about the outer coating, but I've not heard of there being problems.
 
According Norsok standard common requirements for cathodic protection the Chemical composition of aluminum anode materials shall be of the AlZnIn type conforming to table bellow:

ELEMENT MAX % MIN %
Zinc (Zn) 5.5 2.5
Indium (In) 0.040 0.015
Iron (Fe) 0.09
Silicon (Si) 0.10
Copper (Cu) 0.005
Others (Each) 0.02
Aluminium (Al) Remainder
 