My parent’s 40 year old house in Canborough, Ontario, Canada started to shift/ sink for the first noticeable time during the driest part of the summer this year. My assessment was that the large trees adjacent the house (approximately 30-40’ away) dried out the soil (very high clay content) by this end of the house more than the other soil in the vicinity causing uneven settlement due to drying shrinkage of the clay soil. The house has a full basement, strip footings, and CMU foundation walls.
A relative in the foundation repair business suggested helical screw piles or hydraulic push rods as a repair at the 2 corners and the chimney location to push the foundation back into position. I question whether this approach will create “hard points” which won’t move with the rest of the house during subsequent wetting/ drying movement of the rest of the foundations in the future and only create farther problems.
Have a look at the attached pictures. I welcome others suggestions regarding the root cause and any recommended repairs or experiences.
Much Appreciated!
Great spirits have always encountered violent opposition from mediocre minds - Albert Einstein
My parent’s 40 year old house in Canborough, Ontario, Canada started to shift/ sink for the first noticeable time during the driest part of the summer this year. My assessment was that the large trees adjacent the house (approximately 30-40’ away) dried out the soil (very high clay content) by this end of the house more than the other soil in the vicinity causing uneven settlement due to drying shrinkage of the clay soil. The house has a full basement, strip footings, and CMU foundation walls.
A relative in the foundation repair business suggested helical screw piles or hydraulic push rods as a repair at the 2 corners and the chimney location to push the foundation back into position. I question whether this approach will create “hard points” which won’t move with the rest of the house during subsequent wetting/ drying movement of the rest of the foundations in the future and only create farther problems.