See Link. I've been following this since Christmas Eve. It must be very slow moving as the latest news is fours days old.
What amazes me is that the same pipeline had a washout about a dozen years ago. You would think that whatever problem it had it would of been fixed for its entire length after that. I'm also curious on what the cause was (and is). Is it mechanical wear? Bad joints? Hydrogen sulfide damage? That old type Prestressed Concrete Cylinder Pipe (PCCP)?
 
Replies continue below

Recommended for you

according to this: the breakage is actually in almost the exact same place, so it would have been repaired in 2004.

Note, however, there was apparently an even earlier failure in 1978 along the same line: