Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

SIMULTANEOUS INJECTION OF CHLORINE & FERROUS SULPHATE IN THE CONDENSER

Status
Not open for further replies.

powering2002

Electrical
Joined
May 8, 2008
Messages
33
Location
ID
I work at Steam Power Plant 2 x 100 MW. We inject Ferrous Sulphate to the COndenser in order to prevent Condenser from Corrosion. We also inject Chlorine (Sodium HypoChlorite) before the travelling screen to prevent Marine organism from growing up in the Condenser. My Question is Could we inject Chlorine simultaneously with Ferrous Sulphate? Thanks for your attention
 
I assume that this is a brass tubed condenser.
You should only need to add ferrous sulfate periodically.

Do your water conditions change a lot (time of day, time of month, time of year)?
Once you have a good surface film it should be fine. But if the water quality changes a lot then you may need to replenish it more often.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
I suspect that hypochlorite is sufficiently strong an oxidant to take ferrous sulphate (Fe+2) to ferric sulphate (Fe+3). Even ordinary oxygen will do this readily if you wait long enough. So you certainly should not combine them prior to injection!
 