It is customery to use API 5L X 65 grades, A 694 F 60 and 65 grades and A 860 material in the top side piping in offshore industry.
Due to the thickness some of the weld joints require PWHT.
It is also noted that suppliers/manufacturer's of above grades express concern on the Physical (Tensile and Yield values) if PWHT is done on this grades. They say that values will go down when heat treated.
That being the case is it not mandated to ask for physical testing in the simulated heat treated condition.
Does any of Pipe line code specify such requirements?
The material standard does not even address the simulation option in supplimentary requirements?
Are simulation tests asked for in the offshore piping industry?
Due to the thickness some of the weld joints require PWHT.
It is also noted that suppliers/manufacturer's of above grades express concern on the Physical (Tensile and Yield values) if PWHT is done on this grades. They say that values will go down when heat treated.
That being the case is it not mandated to ask for physical testing in the simulated heat treated condition.
Does any of Pipe line code specify such requirements?
The material standard does not even address the simulation option in supplimentary requirements?
Are simulation tests asked for in the offshore piping industry?