Hi Guys,
I'd like to ask you for support to estimate of part life.
Real process:
Two cut-off (hardener tool steel,tested 64HRC) blades cutting the copper wire OD=2mm during serial wire production. V-edge profile blades shearing this wire with constant force and after 15k cycles new blade edge is dulled/blunted.
Is it possible to try estimate life of the blade?
All B.C.s to analysis are known like: temp, force, material etc.
Thanks you for any suggestion.
I'd like to ask you for support to estimate of part life.
Real process:
Two cut-off (hardener tool steel,tested 64HRC) blades cutting the copper wire OD=2mm during serial wire production. V-edge profile blades shearing this wire with constant force and after 15k cycles new blade edge is dulled/blunted.
Is it possible to try estimate life of the blade?
All B.C.s to analysis are known like: temp, force, material etc.
Thanks you for any suggestion.