Nov 16, 2012 #1 glazetm Industrial Joined Jul 17, 2012 Messages 30 Location US __ Tw, Please describe the meaning of this in asme b31.3. Thanks for your help Thanks, Tommy
Nov 16, 2012 #2 EnergyMix Nuclear Joined Oct 15, 2012 Messages 351 Location US It's defined on page 269 of the standard. Do you not have a copy? Upvote 0 Downvote
Nov 16, 2012 #3 Fizza453 Mechanical Joined Jun 22, 2011 Messages 262 Location AE Tommy3021, It is the minimum wall thickness (nominal)of the components joined by butt weld. Nasir Welding Engineer DESCON ENGINEERING LIMITED PAKISTAN Upvote 0 Downvote
Tommy3021, It is the minimum wall thickness (nominal)of the components joined by butt weld. Nasir Welding Engineer DESCON ENGINEERING LIMITED PAKISTAN
Nov 16, 2012 #4 EnergyMix Nuclear Joined Oct 15, 2012 Messages 351 Location US Fizza, you were missing my point. Upvote 0 Downvote
Nov 16, 2012 #5 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,869 Location US Generally speaking min and nom cannot be used interchangeably. Regards, Mike Upvote 0 Downvote
Nov 16, 2012 Thread starter #6 glazetm Industrial Joined Jul 17, 2012 Messages 30 Location US Thanks to you all. EngeryMix your answer helped too. Thanks, Tommy Upvote 0 Downvote