Hi,
There is a metal produced in Brazil, by USIMINAS denominated USI-SAR80T, it is a quenched and tempered metal and it told to be ~similar~ to SA-517, however I do not know to which grade. I have not be able to fit it properly into a specific grade. Could someone help me out?
Here is the metal composition according to the vendor
C - 0.19% max
Si - 0.55% max
Mn - 0.6% - 1.2%
P - 0.030%
S - 0.030%
Nb + V - 0.15% max
B - 0.0060% max
Cr - 0.4% - 1%
Mo - 0.25% - 0.60%
Below is a composition found in a material certificate
C - 0.12 ; Mn-0.95 ; P - 0.018; S-0.005; Cr-0.73; Ni - 0.01 ; Mo - 0.49; Al - 0.043; Nb-0.001; V-0.036; Ti-0.015;Sn-0.001; N-0.042; B - 0.0021; Ca-0.002; Sb-0.001
Kind Regards
victorpbr
There is a metal produced in Brazil, by USIMINAS denominated USI-SAR80T, it is a quenched and tempered metal and it told to be ~similar~ to SA-517, however I do not know to which grade. I have not be able to fit it properly into a specific grade. Could someone help me out?
Here is the metal composition according to the vendor
C - 0.19% max
Si - 0.55% max
Mn - 0.6% - 1.2%
P - 0.030%
S - 0.030%
Nb + V - 0.15% max
B - 0.0060% max
Cr - 0.4% - 1%
Mo - 0.25% - 0.60%
Below is a composition found in a material certificate
C - 0.12 ; Mn-0.95 ; P - 0.018; S-0.005; Cr-0.73; Ni - 0.01 ; Mo - 0.49; Al - 0.043; Nb-0.001; V-0.036; Ti-0.015;Sn-0.001; N-0.042; B - 0.0021; Ca-0.002; Sb-0.001
Kind Regards
victorpbr