I would like to make a slab out of silver oxide powder with the silver applied to a mesh. I was thinking of a cold two stage rolling operation using paper on each side as a web. I am thinking I may need a binder mixed with the silver or sprayed onto the grid. Does anyone have any input on this idea?
 
Replies continue below

Recommended for you

If the mesh is made of, or plated with, something that will bond to silver oxide with just pressure, maybe you have a chance.

I'd be inclined to try sintering the powder to silver- plated screen cloth, with secondary rolling/ calendering only if you need it to flatten out the slabs.



Mike Halloran
NOT speaking for
DeAngelo Marine Exhaust Inc.