Is there a standard for Slip On flange with RTJ Gasket seating face?

Does B 16.5 address this combination?

Rating 1500

Size 4"

Material ASTM A 105



 
bmoorty,
B16.5 ed 2003 shows in top of Table 5, page 64, the slip-on RTJ flange and is listing the 4", 1500# flanges details, including the R39 groove number...
cheers,
gr2vessels
 
bmoorthy,

ASME B16.5-2003 Tables 20 and F20 (Dimensions of Class 1500 Flanges) list dimensions for slip-on flange up to NPS 2 1/2" only. Therefore, a 4"-1500# RTJ SO flange is not a "standard" B16.5 flange.
 
Doki, try turn the page, Table 20 continues the next page. Please also note that bmoorty is looking for RTJ flanges in Slip-on type, which is not very visible on top of Table 5.
cheers,
gr2vessels
 
Class 1500 slip-on flanges that are greater than NPS 2 1/2" are not covered by ASME B16.5. They would be special or non-standard (i.e. ASME VIII-1 Appendix 2 design). Why use a non-standard slip-on flange when standard B16.5 WN or LJ flanges are available?
 
gr2vessels,

What do you expect me to find by turning the page? Does your copy of ASME B16.5 have "B" and "Y" values for slip-on flanges beyond NPS 2 1/2" on Table 20?

Have you looked at the sketches above Table 20? What does it say for slip-ons? Doesn't it say...Slip-on Welding (NPS 1/2 to 2 1/2 Only)?
 