I'd like to revisit this topic yet again.

Previous review:
thread237-9155
thread237-178054
thread237-224692
thread237-32685

DO NOT USE SILICONE SEALANT TO MAKE THE MOTOR WATERTIGHT

Silicone, RTV, or Bathtub Seal/Caulking is not recommended for sealing DC motors

QUESTION 1 - Any further good references about this? Our repair shop said they wouldn't hesitate to use silicon sealant on a dc motor cover plate as long as it is not near Hydrogen sulfide like paper mmill. What is standard repair industry practice?

QUESTION 2 - What are alternative weather proof sealants? Something with thick consistency for example to fill a 1 / 16" gap?

I found the following alternatives, but don't know much about them.
“Urethanes, polyurethanes or elastomeric adhesive sealants are recommended for use around brush type motors.”


Titeseal
Titeseal is the preferred sealant used on waterproof motors to seal fits and bolts. It is non–hardening,
non–silicone. GE#8064200000.”

=====================================
(2B)+(2B)' ?
 
Replies continue below

Recommended for you

One additional important fact that I forgot to mention is that RTV silicones cure by reacting with moisture in the air. They skin-over in minutes but can take days or weeks to cure to any depths greater than 1/4".
 