hi
i need to know exactly the specific heat of silicon steel used in building the transformer cores.
is it same as the (iron/steel) specific heat that is ( 452 J/Kg/K )
thank you
 
Replies continue below

Recommended for you

The typical value of specific heat for Silicon Steel is: Cp=600 J/kg • K
 
Just out of curiosity:

Will it be the same for the steels manufactured in different processes?

hot-rolled steel
grain-oriented steel
high-permeability steel
domain-refined steel

All are/was used in transformer cores.



[red]Failure seldom stops us, it is the fear for failure that stops us - Jack Lemmon[/red]

Make the best use of Eng-Tips.com
Read the Site Policies at FAQ731-376
 
Hi Ralph

In general, the specific heat are different for different alloys. Typical values are as follow:

- Cold rolled steel: Cp= 481 J/kg.K
- Grain-oriented steel: Cp=812 J/kg•K
- High-permeability: Cp= 460 J/kg.K

 
Dear cukt2000