TestBeforeTouch
Electrical
I am an Electrical Engineer looking for some information on the advantages and disadvantages of the different types of silicon bronze alloys for joining bus bars together.
I know that Silicon bronze is a general term that describes various types of copper-silicon alloys manufactured under trade names such as Everdur, Herculoy, Duronze."
The names seem to represent different types of metalurgy. For example,
Everdur = 95% Cu, 4%Si, 1%Mn
Herculoy = 92% Cu, 4%Si, 4 % Zn
Duronze is available in several different compositions.
But I have not been able to find any information on the benefits of one alloy over another.