May 26, 2005 #1 rpmag Automotive Joined Oct 15, 2004 Messages 105 It was suggested that prior to bonding Aluminium panels to a mild steel structure, both of the surfaces should be bead blasted and then treated with silane. Does anyone have any experiences with Silane?