Hello All
Now the situation is this
I have a pressure vessel that has ASTM 321 materail claded.
This vessel is required to be heat treated. User has expressed fear (Verbally)of Sigma Phase formation, but does not prohibit PWHT.
Just to quell his fear and boost the confidence of the customer, i wanted to perform MICRO Examination on a PQRT Piece (The spec calls was to Qualify PQRT using a clad plate-One to One as per the spec) in the CRA Layer (Plate) and the CRA weld.
Our format for test request calls for the specification to be filled up. If there is no test spec and spec for acceptance criteria it will be classified as developmental work, and our project manager will not permit development work. The problem is the acceptance criteria and the analysis method reference standard (Determination of Sigma phase for SS 321 grade material).
On the weld should i check in the undiluted portion (Top 1.5mm). Is presence of Sigma Phase in the area closer to weld (In CRA) a defenite occurance?
In which case i will avoid testing in this area
The filler wire used is 347 grade.
Now the situation is this
I have a pressure vessel that has ASTM 321 materail claded.
This vessel is required to be heat treated. User has expressed fear (Verbally)of Sigma Phase formation, but does not prohibit PWHT.
Just to quell his fear and boost the confidence of the customer, i wanted to perform MICRO Examination on a PQRT Piece (The spec calls was to Qualify PQRT using a clad plate-One to One as per the spec) in the CRA Layer (Plate) and the CRA weld.
Our format for test request calls for the specification to be filled up. If there is no test spec and spec for acceptance criteria it will be classified as developmental work, and our project manager will not permit development work. The problem is the acceptance criteria and the analysis method reference standard (Determination of Sigma phase for SS 321 grade material).
On the weld should i check in the undiluted portion (Top 1.5mm). Is presence of Sigma Phase in the area closer to weld (In CRA) a defenite occurance?
In which case i will avoid testing in this area
The filler wire used is 347 grade.