Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Sieve Analysis and Hydrometer

Status
Not open for further replies.

Shakta

Geotechnical
Joined
Dec 22, 2015
Messages
25
Location
US
As Sieve analysis with hydrometer test ASTM D422 was replaced by D6913 (sieve analysis) and D7928 (hydrometer), how do you present the result. Do you combine both result and present in one grain size distribution plot, or use two separate plots for sieve analysis and hydrometer part. Is there any direction for combining them? Thanks!
 
If you are doing and ASTM show everything required in the ASTM reporting section, if you can do both on one sheet then do it.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top